Hastelloy C276 vs C22 vs B3: How to Choose the Right Nickel Alloy Pipe and Tube

How to choose between Hastelloy C276, C22 and B3 for HCl, oxidizing chlorides and mixed acids, with ASTM B622, B619 and B626 pipe and tube guidance and an RFQ checklist.

Hastelloy C276 vs C22 vs B3: How to Choose Pipe and Tube

Choose Hastelloy B3 (UNS N10675) when the hydrochloric acid stream stays reducing. Choose Hastelloy C22 (UNS N06022) when oxidizing chlorides and crevices drive the risk. Choose Hastelloy C276 (UNS N10276) for mixed acid service where reducing stages dominate, and compare it directly with C22 before you commit.

A material selection guide for engineers, specifiers and nickel alloy pipe and tube buyers. This guide compares Hastelloy C276, Hastelloy C22 and Hastelloy B3 as they are typically shortlisted for seamless and welded nickel alloy pipe and tube, explains what separates the three grades, and shows what to include in an RFQ so that supplier quotations can be compared line by line.

Concentration, peak metal temperature, oxidizing contaminants and where crevices can form decide the answer — not the alloy’s general reputation. [1–3]

Updated: 14 November 2026. Alloy data and product specifications cited in this guide were checked against the Haynes International technical documents listed under Technical references.

Request a Hastelloy Pipe or Tube Quotation

The Three Alloys at a Glance

Use this table to build a shortlist, not to approve a material. It shows the nominal chemistry of each grade and the service condition that usually governs the choice.

AlloyUNSNominal composition (wt. %)What governs the choice
Hastelloy C-276N1027616 Cr, 16 Mo, 4 WReducing strength from high Mo + W; broad mixed-acid tolerance
Hastelloy C-22N0602222 Cr, 13 Mo, 3 WOxidizing margin from high Cr; higher crevice resistance
Hastelloy B-3N106751.5 Cr, 28.5 MoMaximum resistance to pure, reducing HCl

The values above are nominal. All three are nickel-based alloys, and all three are supplied as seamless pipe and tube, welded pipe and welded tube. Acceptance is against the chemical composition limits in the product specification and edition named on the purchase order — not against this table. [1–3]

Pitting resistance equivalents do not rank B3. Indices such as PREN work for chromium-bearing alloys because they assume a passive film. B3 has almost no chromium, so a PREN number for it is meaningless. Compare B3 on measured corrosion rates in your medium, never on a calculated index. [3]

When to Specify B3 for Hydrochloric Acid

Nickel-molybdenum alloys are the standard choice for hydrochloric acid because no stainless steel holds up across the full concentration range. B3 handles all concentrations of pure HCl up to boiling, and it is far more forgiving to weld than the older B2: tighter control of Fe, Cr and Mo slows the formation of harmful Ni4Mo phases in the 600–800 °C range, so as-welded components often enter service without post-weld solution annealing. [3]

The limit is equally sharp. B3 must not see oxidizing species. In Haynes tests in boiling 2.5 wt.% HCl, the corrosion rate of B3 rises steeply once ferric or cupric ions reach roughly 5 × 10-5 — a contamination level that is easy to introduce by accident. Ferric and cupric ions act as cathodic depolarizers, so the rate stops being controlled by the alloy and starts being controlled by the oxidizer.

Treat these as disqualifying signals for B3, not as details to average out:

  • Upstream carbon steel. Iron pickup plus dissolved oxygen generates Fe3+ in the acid.
  • Copper alloy valves, pumps or instruments releasing Cu2+ into the line.
  • Aeration from unblanketed tanks, pump seals or vacuum sections.
  • Recycled or shared acid, or oxidizing cleaning chemicals.

Where any of these are credible, screen C276 and C22 against contaminated-stream data instead. This is also why B3 and the C-type alloys are complements rather than substitutes: chromium is what buys tolerance to oxidizing impurities, and chromium is what B3 deliberately lacks. [3]

Hastelloy C276 vs C22 for Mixed Acids and Oxidizing Chlorides

Both are nickel-chromium-molybdenum alloys with tungsten, so the difference is one of emphasis. C276 carries more molybdenum and tungsten (15–17 % Mo, up to 4.5 % W), which favours reducing acids and high-temperature chloride salts. C22 carries more chromium (20–22.5 %), which provides more margin in oxidizing media — nitric acid, ferric and cupric chloride, wet chlorine, and mixed streams with an oxidizing stage. [1, 2]

Crevice corrosion is where the two separate most often, and where piping specs are usually lost. In Haynes’ 72-hour test in acidified 6 wt.% ferric chloride (ASTM G48), C22 held a critical crevice temperature of 80 °C against 55 °C for C276 — a 25 °C margin that matters at gasket faces, under deposits and in threaded or lap joints. [2]

ASTM G48, acidified 6 wt.% FeCl3, 72 hC-276C-22
Critical pitting temperature (CPT)Above test limitAbove test limit
Critical crevice temperature (CCT)55 °C80 °C

Read the pitting row carefully. Both alloys exceeded the highest temperature used in the test, so pitting does not separate them — and Haynes’ own documents report the C276 figure as either >120 °C or >150 °C depending on the table. Compare grades within a single test series and never transfer a laboratory temperature into a design limit. These are relative rankings under one set of conditions, not permissible operating temperatures. [2]

For mixed-acid piping, work stage by stage: chemistry, temperature and oxidizing/reducing character for normal operation, cleaning and credible upsets. A line that is reducing in the reactor and oxidizing after a caustic wash may need two different alloys.

Can C22 pipe replace C276 in an existing line?

Only as a deliberate material change, never as an interchange. Four items decide it: corrosion data for the actual stream, the design code and its allowable stresses, the product specification, and the welding procedure. C22 is not a drop-in upgrade — it trades reducing-acid margin for oxidizing margin, so a C276 line running hot, concentrated reducing acid can go backwards. [1, 2]

Filler metals differ as well, and mixing them across a joint is a common field error:

Base alloyMatching GTAW / GMAW filler
C-276 (N10276)ERNiCrMo-4
C-22 (N06022)ERNiCrMo-10
B-3 (N10675)ERNiMo-10

Confirm filler selection, interpass control and any post-weld heat treatment through the qualified procedure, the governing code and the service requirements.

Which ASTM Specification Covers the Pipe or Tube

Grade alone does not define the product. Product form, dimensions and wall basis come from the specification, and all three UNS grades appear in all three documents. [4]

ASTM specificationProduct formDetails to state on the order
ASTM B622Seamless pipe and tubePipe size and schedule, or tube OD and wall thickness; length; nominal or minimum wall
ASTM B619/B619MWelded pipePipe size, schedule or required wall, length, applicable class
ASTM B626Welded tubeOD, wall thickness, wall basis, length

For ASME Code construction, the material specification is the SB- route — SB-622 for seamless pipe and tube, SB-619 and SB-626 for the welded forms — and the applicable Code edition governs. Confirm grade and size coverage, delivery condition and inspection requirements against the contract edition, because the edition in force at quotation is not always the edition you will be inspected to. [4]

Four Specification Mistakes That Cost the Most

  1. Quoting a grade without a product specification. “C276 pipe” leaves form, wall basis and inspection undefined, so two suppliers can quote materially different products at the same price.
  2. Specifying B3 for a system it cannot survive. One carbon steel upstream connection is enough to invalidate the selection.
  3. Using C276 out of habit where crevices dominate. Flange faces and tube-to-tubesheet joints are exactly where the 25 °C CCT gap between C276 and C22 is spent.
  4. Replacing an alloy without re-qualifying the weld procedure. Base metal equivalence does not carry over to filler metal and heat input.

What to Include in a Hastelloy Pipe or Tube RFQ

  • Service conditions. Medium, acid concentration range, normal and peak metal temperature, design pressure, known contaminants — plus cleaning chemicals and credible upsets if material selection is part of the enquiry.
  • Grade and dimensions. UNS number, product specification and edition, seamless or welded, class, delivery condition, dimensions, wall basis, lengths, quantities.
  • Inspection and documentation. Heat traceability, material test report or certificate, purchaser-specified examinations. If a corrosion test is required, agree method, specimen condition and acceptance criteria up front.
  • Commercial basis. Availability and lead time, quoted against identical grade, wall basis, delivery condition and inspection scope.

A copy-paste version that gets a usable answer on the first round:

Grade / UNS: e.g. C-276 / N10276
Specification: ASTM B622 (or B619 / B626), edition
Form and size: e.g. 2″ SCH40 seamless, or 25.4 x 1.65 mm welded tube
Wall basis: nominal / minimum
Length and qty:
Delivery condition: solution annealed
Inspection: MTR to EN 10204 3.1, PMI, hydro, eddy current
Medium / temp: e.g. 15% HCl, 80 °C continuous, 110 °C peak
Destination: port or site

This example is an initial RFQ, not a complete purchase specification or a material recommendation for a particular duty. Before order placement, agree the controlling specification edition, wall basis, test scope and acceptance criteria in writing. [4]

Frequently asked questions

Which is better for pure hydrochloric acid: Hastelloy C276 or B3?

B3, provided the acid stays reducing. B3 handles all concentrations of pure HCl up to boiling, while C276 is the fallback once ferric or cupric ions, aeration or oxidizing cleaning chemicals are credible. Screen the actual stream, not the acid name. [3]

When is Hastelloy C22 the better choice than C276?

When the environment is oxidizing — nitric acid, wet chlorine, ferric or cupric chloride — or when crevices dominate the design. In ASTM G48 acidified 6 wt.% ferric chloride, C22 held a critical crevice temperature of 80 °C against 55 °C for C276. [2]

Can C276 replace B3 in hydrochloric acid service?

Treat it as a new material assessment. C276 tolerates oxidizing contaminants far better than B3, but its lower molybdenum-plus-tungsten content means it should be checked against measured corrosion rates for the actual concentration and temperature before any substitution is approved. [1]

Can B3 be welded without post-weld heat treatment?

Often, yes. Compared with B2, B3’s tighter control of Fe, Cr and Mo slows harmful Ni4Mo formation in the 600–800 °C range, so as-welded components frequently enter service without post-weld solution annealing. Confirm through the qualified welding procedure for the actual thickness and service. [3]

What filler metal matches each alloy?

ERNiCrMo-4 for C-276, ERNiCrMo-10 for C-22 and ERNiMo-10 for B-3. Mixing fillers across a joint is a common field error; confirm selection, interpass control and any post-weld heat treatment through the qualified procedure.

What is the difference between ASTM B622, B619 and B626?

B622 covers seamless pipe and tube, B619 welded pipe and B626 welded tube. All three specifications list C-276, C-22 and B-3, so the product form — not the grade — decides which document to cite. State the edition, class (for welded pipe), wall basis and inspection scope on the order. [4]

Is a PREN comparison valid for these three alloys?

Partially. PREN-type indices assume a chromium-bearing passive film, so they can be discussed for C276 and C22 but are meaningless for B3, which has almost no chromium. Compare B3 on measured corrosion rates in the actual medium. [3]

Choose the Grade with a Clear Service Specification

Use this comparison to build a shortlist, then validate the material against the complete operating envelope: fluid chemistry, peak metal temperature, oxidizing contaminants and crevice locations. A clear specification links the grade to its product form, delivery condition, inspection scope and design basis, which is what allows suppliers to quote on the same basis.

Wenzhou Xinzhe supplies seamless nickel alloy tube and pipe alongside austenitic stainless, duplex and super duplex tubing. For a focused material inquiry, send the process medium and composition, design temperature and pressure, pipe or tube dimensions, construction route and required certification. These details let a supplier answer with a technical proposal rather than a bare price.

Request a Hastelloy C276, C22 or B3 quotation

Send the UNS grade, product specification and edition, pipe or tube dimensions with the wall basis, delivery condition, testing scope and certification requirements with your enquiry. If the grade is still open, send the process chemistry and peak metal temperature and our technical team will screen C276, C22 and B3 against your actual service conditions.

Send your RFQ to Wenzhou Xinzhe

Technical references

This guide provides an overview rather than a complete procurement specification. The cited documents identify the basis of the technical discussion; the edition specified by the contract and the governing design requirements control acceptance. HASTELLOY is a registered trademark of Haynes International.

Related product pages

Each linked page lists the sizes, applicable standard and the inspection documents we can supply.

Last reviewed: · Wenzhou Xinzhe Tech Co., Ltd. · Contact the technical team

Share your love