ASTM A790 vs A789 vs A928 Duplex Pipe and Tube Standards
A practical guide to ASTM A790, A789 and A928 duplex stainless steel pipe and tube standards covering scope, manufacturing routes, grades, PREN, testing and ordering.
Most duplex enquiries turn on a specification question before they turn on price: whether A790, A789 or A928 governs the product being bought, what a PREN figure really predicts in chloride service, where 2205 stops being enough and 2507 starts, and why the mechanical property minimums are tied to the solution-annealed condition. The notes in this series work those questions through with the standard clause and the grade limit in view, written for buyers, inspectors and fabricators rather than for a catalogue.
Scope: the austenitic-ferritic grades we supply and write about — 2205 (S32205/S31803), 2304, 329, 255 (S32550), 2507 (S32750), Zeron 100 (S32760) and the lean and hyper-duplex grades such as LDX 2101, LDX 2404 and SAF 2707 HD. Standard-by-standard summaries sit in the Standards library; market, price and trade notes sit in Steel Info & News. This category holds the engineering material between the two.
| Buyer question | Start with | What the note settles |
|---|---|---|
| Which standard governs the product — A790, A789 or A928? | ASTM A790 vs A789 vs A928 | Seamless and welded pipe (A790), tube (A789) and electric-fusion-welded pipe made with filler metal (A928), and which of the three the purchase order has to name. |
| Will duplex survive chlorides and H2S? | Duplex pipes and chloride SCC | Where PREN and the ISO 15156 / NACE MR0175 limits place 2205 and 2507, and the temperature ceilings that decide the answer. |
| What tensile and yield values apply? | Mechanical properties of duplex pipe | A790 and A789 minimum tensile, yield and elongation by grade, and the solution-annealed condition those values apply to. |
| 2205 or 2507 — which do I need? | Duplex vs super duplex | The PREN 40 boundary, the nickel and molybdenum step between the two grades, and the fabrication cost that comes with it. |
| Where is duplex actually used? | Applications and grade comparisons | Service segments where duplex replaces 316L or 904L on wall thickness and life cycle, and where it does not. |
Last reviewed: 10 November 2026 · Wenzhou Xinzhe Tech Co., Ltd.
A practical guide to ASTM A790, A789 and A928 duplex stainless steel pipe and tube standards covering scope, manufacturing routes, grades, PREN, testing and ordering.

Duplex resists chloride SCC better than 304L/316L but is not immune. Compare 2205 and super duplex, PREN, weld condition and ISO 15156 sour-service limits.
Mechanical Properties of Duplex and Super Duplex Stainless Steel Pipe ASTM A790/A790M-24 specifies minimum…

Compare duplex 2205 (S32205) and super duplex 2507 (S32750) stainless steel pipe by chemistry, PREN, specified strength, corrosion resistance, welding requirements and material selection.

Where duplex seamless pipes are used, how standard duplex UNS S32205 compares with super duplex UNS S32750/S32760 (PREN, chemistry, mechanical properties), and the market and technology trends shaping future demand.